Ingredient Instruction:
1.Solution: inorganic bond water solution, transparent
2.PH: 10~12
3.Main Ingredients & Content: TiO2 (0.2~0.5%), SiO2 (0.5~1%), H2O (97.5~98.8%), Others (0.5~1%)
4.Viscosity: 800~1000mpa.s
5.Average Grain-size: 10~15nm
6.Suggested volume for the spray coating one layer: 10~30(ml/m2)